Customize Consent Preferences

We use cookies to help you navigate efficiently and perform certain functions. You will find detailed information about all cookies under each consent category below.

The cookies that are categorized as "Necessary" are stored on your browser as they are essential for enabling the basic functionalities of the site. ... 

Always Active

Necessary cookies are required to enable the basic features of this site, such as providing secure log-in or adjusting your consent preferences. These cookies do not store any personally identifiable data.

No cookies to display.

Functional cookies help perform certain functionalities like sharing the content of the website on social media platforms, collecting feedback, and other third-party features.

No cookies to display.

Analytical cookies are used to understand how visitors interact with the website. These cookies help provide information on metrics such as the number of visitors, bounce rate, traffic source, etc.

No cookies to display.

Performance cookies are used to understand and analyze the key performance indexes of the website which helps in delivering a better user experience for the visitors.

No cookies to display.

Advertisement cookies are used to provide visitors with customized advertisements based on the pages you visited previously and to analyze the effectiveness of the ad campaigns.

No cookies to display.

MENU

Weld Purging Systems - will not over inflate or burst

Quick Purge Weld Purging Systems for Pipes, Pipelines and Tube Welding

We recently had an order from a European customer in the LNG industry who was using a competitive inflatable weld purging system.

While welding large diameter stainless steel pipes on site, these competitive systems were bursting due to over inflation, causing the complete loss of valuable welds due to the entrance of atmospheric air. This in turn led to dramatic oxidation and metallurgical defects, which resulted in an extremely costly cut out and re-weld.

Having lost welds, the project suffered delays, additional costs and the Welding Engineer was looking at other options, including filling the entire pipes with argon, which would have had health and safety implications as well as a very high additional expense.

Upon browsing the HFT ® website and reading White Paper 27 – Weld Purging on LNG Projects, he discovered the QuickPurge ® System, which was developed in association with Mitsui Babcock, especially for large diameter stainless steel pipes.

The QuickPurge ® System suits pipe diameters from 6 – 96” and is fitted as standard with a special pressure relief valve, PurgeGate ®, which regulates the gas flow in such a way, that it will never burst due to over inflation.

 Weld Purging: Quick Purge Systems

This state of the art system is also manufactured with RootGlo ®, a central band that glows inside a dark pipe allowing the system to be aligned correctly, so the two sealing dams are a perfect distance away from the weld zone.

The customer contacted the HFT ® HQ, was given more technical information about the QuickPurge ® and was put in touch with his nearest Exclusive Distributor, who stocks our QuickPurge ® Systems.

After a satisfactory demonstration by the Distributor the very next day, the customer tried everyway that he could to over inflate the system and burst it, but found he couldn't. He immediately purchased his replacement products and was able to continue the job without any further loss of time.

To read the White Paper in full, please click here.


STILL HAVEN’T FOUND WHAT YOU’RE LOOKING FOR?

Contact us with a question using the form here. Alternatively give us a call.
Contact Form

By submitting this inquiry, you agree to subscribe to receive updates, news, and exclusive offers from Huntingdon Fusion Techniques (HFT). You can opt-out at any time.

Copyright © Huntingdon Fusion Techniques HFT®.  All Rights Reserved..
Privacy Policy