We use cookies to help you navigate efficiently and perform certain functions. You will find detailed information about all cookies under each consent category below.
The cookies that are categorized as "Necessary" are stored on your browser as they are essential for enabling the basic functionalities of the site. ...
Necessary cookies are required to enable the basic features of this site, such as providing secure log-in or adjusting your consent preferences. These cookies do not store any personally identifiable data.
Functional cookies help perform certain functionalities like sharing the content of the website on social media platforms, collecting feedback, and other third-party features.
Analytical cookies are used to understand how visitors interact with the website. These cookies help provide information on metrics such as the number of visitors, bounce rate, traffic source, etc.
Performance cookies are used to understand and analyze the key performance indexes of the website which helps in delivering a better user experience for the visitors.
Advertisement cookies are used to provide visitors with customized advertisements based on the pages you visited previously and to analyze the effectiveness of the ad campaigns.
It is reported by TWI (The Welding Institute) that Nickel alloys can suffer with porosity if Nitrogen is present in the purge environment with a concentration of as little as 0.025% (250 ppm).
As a result, it is necessary to back purge Nickel alloy joints to better than 80 ppm Oxygen.
For this purpose, it would be wise for all operators to specify that a “Weld Purge Monitor” should be used to check the purge gas quality prior to welding.
Standard “Wet Cell” Weld Purge Monitors are accurate to 100 ppm, however there are now low cost, entry level, Weld Purge Monitors available with zirconia sensors that are very accurate to 10 ppm.